General
Mechanical
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Bending Fatigue Strength | 70.0 MPa Show Material materials with Bending Fatigue Strength of 70.0 MPa | T5 | AA Standards | ||
Compressive modulus | 69.7 MPa Show Material materials with Compressive modulus of 69.7 MPa | T5 | |||
Elastic modulus | 69.0 GPa Show Material materials with Elastic modulus of 69.0 GPa | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | ||
69 GPa Show Material materials with Elastic modulus of 69 GPa | T5 | ||||
Elongation | -195 °C | 28 % Show Material materials with Elongation of 28 % | T5 | Elongation in 50 mm | |
-80 °C | 24 % Show Material materials with Elongation of 24 % | T5 | Elongation in 50 mm | ||
7.0 % Show Material materials with Elongation of 7.0 % | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | A100 | ||
8.0 % Show Material materials with Elongation of 8.0 % | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | A50 | ||
11.0 % Show Material materials with Elongation of 11.0 % | T5 | ||||
12.0 % Show Material materials with Elongation of 12.0 % | T5 | AA Standards | A50 | ||
0 °C | 23 % Show Material materials with Elongation of 23 % | T5 | Elongation in 50 mm | ||
24 °C | 22 % Show Material materials with Elongation of 22 % | T5 | Elongation in 50 mm | ||
100 °C | 18 % Show Material materials with Elongation of 18 % | T5 | Elongation in 50 mm | ||
150 °C | 20 % Show Material materials with Elongation of 20 % | T5 | Elongation in 50 mm | ||
205 °C | 40 % Show Material materials with Elongation of 40 % | T5 | Elongation in 50 mm | ||
260 °C | 75 % Show Material materials with Elongation of 75 % | T5 | Elongation in 50 mm | ||
315 °C | 80 % Show Material materials with Elongation of 80 % | T5 | Elongation in 50 mm | ||
370 °C | 105 % Show Material materials with Elongation of 105 % | T5 | Elongation in 50 mm | ||
Fatigue strength | 69 MPa Show Material materials with Fatigue strength of 69 MPa | T5 | fo 5x10⁸ cycles | ||
Hardness, Brinell | 60.0 [-] Show Material materials with Hardness, Brinell of 60.0 [-] | T5 | AA Standards | ||
60.0 [-] Show Material materials with Hardness, Brinell of 60.0 [-] | T5 | 500 kg load, 10 mm ball | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | |||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | |||
Shear modulus | 26.0 - 26.5 GPa Show Material materials with Shear modulus of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | |||
Shear strength | 117.0 MPa Show Material materials with Shear strength of 117.0 MPa | T5 | |||
Tensile strength | -195 °C | 255 MPa Show Material materials with Tensile strength of 255 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture | |
-80 °C | 200 MPa Show Material materials with Tensile strength of 200 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture | ||
145.0 MPa Show Material materials with Tensile strength of 145.0 MPa | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | |||
150.0 MPa Show Material materials with Tensile strength of 150.0 MPa | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | |||
180.0 MPa Show Material materials with Tensile strength of 180.0 MPa | T5 | ||||
185.0 MPa Show Material materials with Tensile strength of 185.0 MPa | T5 | AA Standards | |||
0 °C | 193 MPa Show Material materials with Tensile strength of 193 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture | ||
24 °C | 185 MPa Show Material materials with Tensile strength of 185 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture | ||
100 °C | 165 MPa Show Material materials with Tensile strength of 165 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture | ||
150 °C | 138 MPa Show Material materials with Tensile strength of 138 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture | ||
205 °C | 62 MPa Show Material materials with Tensile strength of 62 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture | ||
260 °C | 31 MPa Show Material materials with Tensile strength of 31 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture | ||
315 °C | 22 MPa Show Material materials with Tensile strength of 22 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture | ||
370 °C | 16 MPa Show Material materials with Tensile strength of 16 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture | ||
Yield strength | -196 °C | 165 MPa Show Material materials with Yield strength of 165 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture, RP02 | |
-80 °C | 152 MPa Show Material materials with Yield strength of 152 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture, RP02 | ||
-28 °C | 152 MPa Show Material materials with Yield strength of 152 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture, RP02 | ||
105.0 MPa Show Material materials with Yield strength of 105.0 MPa | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | RP02 | ||
110.0 MPa Show Material materials with Yield strength of 110.0 MPa | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | RP02 | ||
140.0 MPa Show Material materials with Yield strength of 140.0 MPa | T5 | ||||
145.0 MPa Show Material materials with Yield strength of 145.0 MPa | T5 | AA Standards | RP02 | ||
24 °C | 145 MPa Show Material materials with Yield strength of 145 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture, RP02 | ||
100 °C | 138 MPa Show Material materials with Yield strength of 138 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture, RP02 | ||
149 °C | 124 MPa Show Material materials with Yield strength of 124 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture, RP02 | ||
204 °C | 45 MPa Show Material materials with Yield strength of 45 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture, RP02 | ||
260 °C | 24 MPa Show Material materials with Yield strength of 24 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture, RP02 | ||
316 °C | 17 MPa Show Material materials with Yield strength of 17 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture, RP02 | ||
371 °C | 14 MPa Show Material materials with Yield strength of 14 MPa | T5 | up to 10000 h at temperature, at 35 MPa/min to yield strength and then at strain rate of 5%/min to fracture, RP02 |
Thermal
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Coefficient of thermal expansion | 2.3e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3e-05 1/K | T5 | ||
20 °C | 2.3399999999999996e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | |
100 °C | 2.3399999999999996e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | |
Melting point | 615.0 - 655.0 °C Show Material materials with Melting point of 615.0 - 655.0 °C | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | |
620.0 °C Show Material materials with Melting point of 620.0 °C | T5 | |||
Specific heat capacity | 900.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 J/(kg·K) | T5 | ||
Thermal conductivity | 193.0 - 218.0 W/(m·K) Show Material materials with Thermal conductivity of 193.0 - 218.0 W/(m·K) | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | |
200.0 W/(m·K) Show Material materials with Thermal conductivity of 200.0 W/(m·K) | T5 |
Electrical
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Electrical conductivity | 29000000.0 - 34000000.0 S/m Show Material materials with Electrical conductivity of 29000000.0 - 34000000.0 S/m | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | |
32000000 S/m Show Material materials with Electrical conductivity of 32000000 S/m | T5 | Typical value | ||
Electrical resistivity | 2.94e-08 - 3.45e-08 Ω·m Show Material materials with Electrical resistivity of 2.94e-08 - 3.45e-08 Ω·m | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | |
3.2e-08 Ω·m Show Material materials with Electrical resistivity of 3.2e-08 Ω·m | T5 | Typical value | ||
Specific Electrical conductivity | 55.0 % IACS Show Material materials with Specific Electrical conductivity of 55.0 % IACS | T5 | Typical/Derived value |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 97.5 - 99.4 % Show Material materials with Aluminium of 97.5 - 99.4 % | T5 | |
Chromium | 0.1 % Show Material materials with Chromium of 0.1 % | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 |
Copper | 0.1 % Show Material materials with Copper of 0.1 % | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 |
Iron | 0.35 % Show Material materials with Iron of 0.35 % | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 |
0.35 % Show Material materials with Iron of 0.35 % | T5 | ||
Magnesium | 0.45 - 0.9 % Show Material materials with Magnesium of 0.45 - 0.9 % | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 |
Other | 0.15 % Show Material materials with Other of 0.15 % | T5 | |
Silicon | 0.2 - 0.6 % Show Material materials with Silicon of 0.2 - 0.6 % | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 |
Titanium | 0.1 % Show Material materials with Titanium of 0.1 % | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | T5 | AA Standards, ASTM B221, ASTM B241, ASTM B345 |
Technological properties
Property | ||
---|---|---|
Brazing | general: possible with commercial processes and methods | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: poor (T1, T4), sufficient (T5, T452, T6, T83, T831, T832) | |
Workability | general (condition): acceptable (T1, T4, T5, T452), poor(T6, T83, T831, T832) |