See where AA 6063 T8 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2.7 g/cm³ at 23 °C
Coefficient of thermal expansion
α2.3E-5 1/K at 23 °C
Melting point
Tm620 °C
Specific heat capacity
cp900 J/(kg·K) at 23 °C
Thermal conductivity
λ200 W/(m·K) at 23 °C
Electrical conductivity
σel2.10E+7 - 3.40E+7 S/m at 23 °C
Typical for Wrought 6000 Series Aluminium
Electrical resistivity
ρel2.9E-8 - 5E-8 Ω·m at 23 °C
Typical for Wrought 6000 Series Aluminium
Element
Weight %
Comment
97.5 - 99.4 %
0.45 - 0.9 %
0.2 - 0.6 %
0 - 0.1 %
0 - 0.1 %
Workability
Excellent workability.
This material data has been provided by MakeItFrom.com.