Density ρ
2.7 g/cm³ at 20 °C
Elastic modulus E
72 GPa at 20 °C
Elongation A
9.2 % at 20 °C
Tensile strength Rm
320 MPa at 20 °C
Yield strength YS
230 MPa at 20 °C
Coefficient of thermal expansion α
2.3E-5 1/K at 20 °C
Melting point Tm
580 °C
Specific heat capacity cp
890 J/(kg·K) at 20 °C
Thermal conductivity λ
209.99 - 219.99 W/(m·K) at 20 °C
Element
Weight %
Comment
95.2 - 98.3 %
0.7 - 1.3 %
0.6 - 1.2 %
0.4 - 1 %