Standards

Chemical composition

Element Weight %
Al 99.6 — 100.0
Fe 0.35
Si 0.25
Cu 0.05
Zn 0.05
V 0.05
Ti 0.03
Mn 0.03
Mg 0.03

Properties

General information

Density [ ρ ]

2.70 g/cm³

Mechanical

Elastic modulus [ E ]

69.00 GPa

Elongation [ A ]

7.70 %

Elongation A50 [ A50 ]

1.00—12.00 %

Hardness, Brinell [ HB ]

26.00 [-]

Tensile strength [ Rm ]

85.00—100.00 MPa

Yield strength [ YS ]

84.00 MPa

Yield strength Rp0.2 [ Rp0.2 ]

70.00—90.00 MPa

Thermal

Coefficient of thermal expansion [ α ]

2.4E-5 1/K

Melting point [ Tm ]

650 °C

Specific heat capacity [ cp ]

900.00 J/(kg·K)

Thermal conductivity [ λ ]

230.00 W/(m·K)

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Alukey, Ingenieurbüro Dr. Hesse
This material data has been provided by Alukey, Ingenieurbüro Dr. Hesse
MakeItFrom, Iron Boar Labs Ltd.
This material data has been provided by MakeItFrom, Iron Boar Labs Ltd.

Download material data

Material data to download as .xlsx and .pdf file.

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MITF380 to find materials similar to AA 1060 H14.