Chemical composition

Element Weight %
Fe 70.7 — 78.0
Cr 16.0 — 18.0
Ni 6.0 — 8.0
Mn 0.0 — 2.0
Si 0.0 — 1.0
P 0.0 — 0.045
C 0.0 — 0.03
S 0.0 — 0.03

Properties

General information

Density [ ρ ]

7.80 g/cm³

Mechanical

Elastic modulus [ E ]

220.00 GPa

Elongation [ A ]

46.00 %

Tensile strength [ Rm ]

790.00 MPa

Yield strength [ YS ]

400.00 MPa

Thermal

Coefficient of thermal expansion [ α ]

1.2E-5 1/K

Specific heat capacity [ cp ]

450.00 J/(kg·K)

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
MakeItFrom, Iron Boar Labs Ltd.
This material data has been provided by MakeItFrom, Iron Boar Labs Ltd.

Suppliers of Steel

The following suppliers might provide 1/16-Hard AISI 301L:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MITF4 to find materials similar to 1/16-Hard AISI 301L.