Properties

Electrical

Electrical conductivity σel

6.96E+7 S/m at 20 °C

General

Density ρ

17 g/cm³ at 20 °C

Mechanical

Elastic modulus E

110 GPa at 20 °C

Elongation A

8.5 % at 20 °C

Tensile strength Rm

1000 MPa at 20 °C

Yield strength YS

790 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.3E-5 1/K at 20 °C

Melting point Tm

930 °C

Specific heat capacity cp

170 J/(kg·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Au

70.5 - 72.5 %

Cu

13.5 - 15.5 %

Pt

8 - 9 %

Ag

4 - 5 %

Zn

0.7 - 1.3 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Find a supplier

We can help you find a supplier of Age Hardened And Annealed ASTM B541

We will evaluate your request and get back to you soon.