Density ρ
8.2 g/cm³ at 20 °C
Elastic modulus E
190 GPa at 20 °C
Elongation A
10 % at 20 °C
Tensile strength Rm
1800 MPa at 20 °C
Yield strength YS
1820 MPa at 20 °C
Coefficient of thermal expansion α
1.3E-5 1/K at 20 °C
Specific heat capacity cp
440 J/(kg·K) at 20 °C
Element
Weight %
Comment
66.3 - 71.1 %
17 - 19 %
7 - 8.5 %
4.6 - 5.2 %
0.3 - 0.5 %
This material data has been provided by MakeItFrom.com.