General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.2 g/cm³ Show Material materials with Density of 8.2 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 GPa Show Material materials with Elastic modulus of 190 GPa | |
Elongation | 23.0 °C | 18 % Show Material materials with Elongation of 18 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Maraging Steel |
Tensile strength | 23.0 °C | 1030 MPa Show Material materials with Tensile strength of 1030 MPa | |
Yield strength | 23.0 °C | 760 MPa Show Material materials with Yield strength of 760 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K | |
Melting point | 1425 - 1505 °C Show Material materials with Melting point of 1425 - 1505 °C | Typical for Maraging Steel | |
Specific heat capacity | 23.0 °C | 440 J/(kg·K) Show Material materials with Specific heat capacity of 440 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 20 - 25 W/(m·K) Show Material materials with Thermal conductivity of 20 - 25 W/(m·K) | Typical for Maraging Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 - 0.15 % Show Material materials with Aluminium of 0.05 - 0.15 % |
Boron | 0 - 3E-3 % Show Material materials with Boron of 0 - 3E-3 % |
Calcium | 0 - 0.05 % Show Material materials with Calcium of 0 - 0.05 % |
Carbon | 0 - 0.03 % Show Material materials with Carbon of 0 - 0.03 % |
Cobalt | 8.5 - 9.5 % Show Material materials with Cobalt of 8.5 - 9.5 % |
Iron | 65 - 68.4 % Show Material materials with Iron of 65 - 68.4 % |
Manganese | 0 - 0.1 % Show Material materials with Manganese of 0 - 0.1 % |
Molybdenum | 4.6 - 5.2 % Show Material materials with Molybdenum of 4.6 - 5.2 % |
Nickel | 18 - 19 % Show Material materials with Nickel of 18 - 19 % |
Phosphorus | 0 - 0.01 % Show Material materials with Phosphorus of 0 - 0.01 % |
Silicon | 0 - 0.1 % Show Material materials with Silicon of 0 - 0.1 % |
Sulfur | 0 - 0.01 % Show Material materials with Sulfur of 0 - 0.01 % |
Titanium | 0.5 - 0.8 % Show Material materials with Titanium of 0.5 - 0.8 % |
Zirconium | 0 - 0.02 % Show Material materials with Zirconium of 0 - 0.02 % |