1060-H24 Aluminium

Chemical composition

Element Weight %
Al 99.6100.0
Fe 0.00.35
Si 0.00.25
V 0.00.05
Zn 0.00.05
Cu 0.00.05
Mn 0.00.03
Ti 0.00.03
Mg 0.00.03


Electrical conductivity, σ
3.6E+8 S/m
General information
Density, ρ
2.70 g/cm³
Elastic modulus, E
69.00 GPa
Elongation, A
1.20 %
Tensile strength, Rm
100.00 MPa
Yield strength, YS
81.00 MPa
Coefficient of thermal expansion, α
2.4E-5 1/K
Melting point, Tm
650 °C
Specific heat capacity, cp
900.00 J/(kg·K)
Thermal conductivity, λ
230.00 W/(m·K)
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
MakeItFrom, Iron Boar Labs Ltd.
This material data has been provided by MakeItFrom, Iron Boar Labs Ltd.


There is currently no supplier information available for this material. No problem, though — we can help you source this or any other material of your interest.

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to to find materials similar to 1060-H24 Aluminium.