Density ρ
4.4 g/cm³ at 20 °C
Elastic modulus E
120 GPa at 20 °C
Elongation A
11 % at 20 °C
Tensile strength Rm
1010 MPa at 20 °C
Yield strength YS
920 MPa at 20 °C
Coefficient of thermal expansion α
8.9E-6 1/K at 20 °C
Melting point Tm
1650 °C
Specific heat capacity cp
560 J/(kg·K) at 20 °C
Thermal conductivity λ
6.8 W/(m·K) at 20 °C
Element
Weight %
Comment
87.4 - 91 %
5.5 - 6.8 %
3.5 - 4.5 %
0.4 %
0.4 %
This material data has been provided by MakeItFrom.com.