Chemical composition

Element Weight %
Al 99.0 — 100.0
Fe 0.0 — 1.0
Si 0.0 — 1.0
Cu 0.05 — 0.2
Other 0.0 — 0.15
Zn 0.0 — 0.1
Mn 0.0 — 0.05

Properties

Electrical

Electrical conductivity

[ σel ]

Electrical conductivity

3.42E+8 S/m

General information

Density

[ ρ ]

Density

2.80 g/cm³

Mechanical

Elastic modulus

[ E ]

Elastic modulus

69.00 GPa

Tensile strength

[ Rm ]

Tensile strength

86.00 MPa

Yield strength

[ YS ]

Yield strength

29.00 MPa

Thermal

Coefficient of thermal expansion

[ α ]

Coefficient of thermal expansion

2.4E-5 1/K

Melting point

[ Tm ]

Melting point

640 °C

Specific heat capacity

[ cp ]

Specific heat capacity

900.00 J/(kg·K)

Thermal conductivity

[ λ ]

Thermal conductivity

220.00 W/(m·K)

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
MakeItFrom, Iron Boar Labs Ltd.
This material data has been provided by MakeItFrom, Iron Boar Labs Ltd.

Suppliers of Wrought Aluminium

The following suppliers might provide 1100-H113 Aluminium:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MITF47 to find materials similar to 1100-H113 Aluminium.