Properties

General

Density

ρ

8.9 g/cm³ at 20 °C

Mechanical

Elastic modulus

E

180 GPa at 20 °C

Elongation

A

34 % at 20 °C

Tensile strength

Rm

640 MPa at 20 °C

Yield strength

YS

310 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

1.4E-5 1/K at 20 °C

Melting point

Tm

1320 °C

Specific heat capacity

cp

420 J/(kg·K) at 20 °C

Thermal conductivity

λ

18 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

5.63E+7 S/m at 20 °C

Chemical properties

Element

Weight %

Comment

Ni

63 - 70.4 %

Cu

27 - 33 %

Al

2.3 - 3.2 %

Ti

0.35 - 0.85 %

C

0 - 0.18 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.