Annealed R31537 Cobalt

.XLSX
.PDF
Save

Properties

Electrical

Electrical conductivity σel

1.16E+7 S/m at 20 °C

General

Density ρ

8.4 g/cm³ at 20 °C

Mechanical

Elastic modulus E

210 GPa at 20 °C

Elongation A

23 % at 20 °C

Tensile strength Rm

1030 MPa at 20 °C

Yield strength YS

590 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.3E-5 1/K at 20 °C

Specific heat capacity cp

470 J/(kg·K) at 20 °C

Thermal conductivity λ

13 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Co

58.9 - 69 %

Cr

26 - 30 %

Mo

5 - 7 %

Si

0 - 1 %

Ni

0 - 1 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.