This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.

Customize your search with filters

Contact suppliers of this material now

Korea, Republic of

Switzerland

AZ63A-F Magnesium

.XLSX
.PDF
Save

Properties

General

Density ρ

2 g/cm³ at 20 °C

Mechanical

Elastic modulus E

49 GPa at 20 °C

Elongation A

4.3 % at 20 °C

Tensile strength Rm

190 MPa at 20 °C

Yield strength YS

81 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.6E-5 1/K at 20 °C

Melting point Tm

450 °C

Specific heat capacity cp

980 J/(kg·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Mg

88.6 - 92.1 %

Al

5.3 - 6.7 %

Zn

2.5 - 3.5 %

Mn

0.15 - 0.35 %

Si

0 - 0.3 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.