See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ7.8 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.5E-5 1/K at 23 °C
Melting point
Tm1400 °C
Specific heat capacity
cp500 J/(kg·K) at 23 °C
Thermal conductivity
λ16 W/(m·K) at 23 °C
Electrical resistivity
ρel8.5E-7 Ω·m at 23 °C
Typical for Austenitic Stainless Steel
Element
Weight %
Comment
58 - 68.5 %
19 - 24 %
11 - 15 %
0 - 0.2 %
0 - 2 %
This material data has been provided by MakeItFrom.com.