General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.4 g/cm³ Show Material materials with Density of 8.4 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 230 GPa Show Material materials with Elastic modulus of 230 GPa |
Elongation | 23.0 °C | 1.2 % Show Material materials with Elongation of 1.2 % |
Tensile strength | 23.0 °C | 1740 MPa Show Material materials with Tensile strength of 1740 MPa |
Yield strength | 23.0 °C | 1110 MPa Show Material materials with Yield strength of 1110 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K |
Specific heat capacity | 23.0 °C | 430 J/(kg·K) Show Material materials with Specific heat capacity of 430 J/(kg·K) |
Chemical properties
Property | Value |
---|---|
Boron | 0 - 1E-3 % Show Material materials with Boron of 0 - 1E-3 % |
Carbon | 0 - 0.15 % Show Material materials with Carbon of 0 - 0.15 % |
Chromium | 18.5 - 21.5 % Show Material materials with Chromium of 18.5 - 21.5 % |
Cobalt | 39 - 42 % Show Material materials with Cobalt of 39 - 42 % |
Iron | 7.6 - 20 % Show Material materials with Iron of 7.6 - 20 % |
Manganese | 1 - 2 % Show Material materials with Manganese of 1 - 2 % |
Molybdenum | 6.5 - 7.5 % Show Material materials with Molybdenum of 6.5 - 7.5 % |
Nickel | 15 - 18 % Show Material materials with Nickel of 15 - 18 % |
Phosphorus | 0 - 0.02 % Show Material materials with Phosphorus of 0 - 0.02 % |
Silicon | 0 - 1.2 % Show Material materials with Silicon of 0 - 1.2 % |
Sulfur | 0 - 0.015 % Show Material materials with Sulfur of 0 - 0.015 % |