General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 10 g/cm³ Show Material materials with Density of 10 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 210 GPa Show Material materials with Elastic modulus of 210 GPa |
Elongation | 23.0 °C | 35 % Show Material materials with Elongation of 35 % |
Tensile strength | 23.0 °C | 1900 MPa Show Material materials with Tensile strength of 1900 MPa |
Yield strength | 23.0 °C | 1600 MPa Show Material materials with Yield strength of 1600 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K |
Melting point | 1330 °C Show Material materials with Melting point of 1330 °C | |
Specific heat capacity | 23.0 °C | 390 J/(kg·K) Show Material materials with Specific heat capacity of 390 J/(kg·K) |
Thermal conductivity | 23.0 °C | 9.4 W/(m·K) Show Material materials with Thermal conductivity of 9.4 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbon | 0.05 - 0.15 % Show Material materials with Carbon of 0.05 - 0.15 % |
Chromium | 19 - 21 % Show Material materials with Chromium of 19 - 21 % |
Cobalt | 46.4 - 57 % Show Material materials with Cobalt of 46.4 - 57 % |
Iron | 0 - 3 % Show Material materials with Iron of 0 - 3 % |
Manganese | 1 - 2 % Show Material materials with Manganese of 1 - 2 % |
Nickel | 9 - 11 % Show Material materials with Nickel of 9 - 11 % |
Phosphorus | 0 - 0.04 % Show Material materials with Phosphorus of 0 - 0.04 % |
Silicon | 0 - 0.4 % Show Material materials with Silicon of 0 - 0.4 % |
Sulfur | 0 - 0.03 % Show Material materials with Sulfur of 0 - 0.03 % |
Tungsten | 14 - 16 % Show Material materials with Tungsten of 14 - 16 % |