General

Density

ρ

17 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

190 GPa at 23 °C

Show Tantalum materials with Elastic modulus of 190 GPa at 23 °C

Elongation

A

1.2 % at 23 °C

Show Tantalum materials with Elongation of 1.2 % at 23 °C

Poisson's ratio

ν

0.34 [-] at 23 °C

Show Tantalum materials with Poisson's ratio of 0.34 [-] at 23 °C

Typical for Tantalum

Shear modulus

G

69 GPa at 23 °C

Show Tantalum materials with Shear modulus of 69 GPa at 23 °C

Typical for Tantalum

Tensile strength

Rm

550 MPa at 23 °C

Show Tantalum materials with Tensile strength of 550 MPa at 23 °C

Yield strength

YS

400 MPa at 23 °C

Show Tantalum materials with Yield strength of 400 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

6.5E-6 1/K at 23 °C

Melting point

Tm

2996 °C

Typical for Tantalum

Specific heat capacity

cp

140 J/(kg·K) at 23 °C

Thermal conductivity

λ

52 - 57 W/(m·K) at 23 °C

Typical for Tantalum

Chemical properties

Element

Weight %

Comment

Ta

99.8 - 100 %

C

0 - 0.01 %

H

0 - 1.5E-3 %

Fe

0 - 0.01 %

Mo

0 - 0.02 %

More

This material data has been provided by MakeItFrom.com.