Electrical conductivity σel
3.60E+8 S/m at 20 °C
Density ρ
2.7 g/cm³ at 20 °C
Elastic modulus E
69 GPa at 20 °C
Tensile strength Rm
100 MPa at 20 °C
Coefficient of thermal expansion α
2.4E-5 1/K at 20 °C
Melting point Tm
650 °C
Specific heat capacity cp
900 J/(kg·K) at 20 °C
Thermal conductivity λ
230 W/(m·K) at 20 °C
Element
Weight %
Comment
99.5 - 100 %
0 - 0.01 %
0 - 0.05 %
0 - 0.02 %
0 - 0.02 %