See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueCondition

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

H22

Mechanical

PropertyValueConditionComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

H22

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 1000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 1000 Series Aluminium

Shear modulus

25.9 GPa

Show Material materials with Shear modulus of 25.9 GPa

Typical for Wrought 1000 Series Aluminium

Tensile strength

93.0 MPa

Show Material materials with Tensile strength of 93.0 MPa

H22

Thermal

PropertyValueCondition

Coefficient of thermal expansion

2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K

H22

Melting point

650.0 °C

Show Material materials with Melting point of 650.0 °C

H22

Specific heat capacity

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

H22

Thermal conductivity

230.0 W/(m·K)

Show Material materials with Thermal conductivity of 230.0 W/(m·K)

H22

Electrical

PropertyValueComment

Electrical conductivity

33000000.0 - 38000000.0 S/m

Show Material materials with Electrical conductivity of 33000000.0 - 38000000.0 S/m

Typical for Wrought 1000 Series Aluminium

Electrical resistivity

2.7e-08 - 3e-08 Ω·m

Show Material materials with Electrical resistivity of 2.7e-08 - 3e-08 Ω·m

Typical for Wrought 1000 Series Aluminium

Chemical properties

PropertyValueCondition

Aluminium

99.5 - 100.0 %

Show Material materials with Aluminium of 99.5 - 100.0 %

H22

Boron

0.05 %

Show Material materials with Boron of 0.05 %

H22

Chromium

0.01 %

Show Material materials with Chromium of 0.01 %

H22

Copper

0.05 %

Show Material materials with Copper of 0.05 %

H22

Gallium

0.03 %

Show Material materials with Gallium of 0.03 %

H22

Iron

0.4 %

Show Material materials with Iron of 0.4 %

H22

Manganese

0.01 %

Show Material materials with Manganese of 0.01 %

H22

Other

0.1 %

Show Material materials with Other of 0.1 %

H22

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

H22

Titanium

0.02 %

Show Material materials with Titanium of 0.02 %

H22

Vanadium

0.02 %

Show Material materials with Vanadium of 0.02 %

H22

Zinc

0.05 %

Show Material materials with Zinc of 0.05 %

H22

Technological properties

Property
Brazing

Excellent

Workability

Excellent workability.