Density
ρ8.4 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.9E-5 1/K at 23 °C
Melting point
Tm980 °C
Specific heat capacity
cp380 J/(kg·K) at 23 °C
Thermal conductivity
λ45 W/(m·K) at 23 °C
Element
Weight %
Comment
57 - 61 %
24.2 - 32 %
11 - 13.5 %
0 - 0.25 %
0 - 0.1 %