201.0-T4 Aluminium

.XLSX
.PDF
Save

Properties

General

Density ρ

3.1 g/cm³ at 20 °C

Mechanical

Elastic modulus E

71 GPa at 20 °C

Elongation A

20 % at 20 °C

Tensile strength Rm

370 MPa at 20 °C

Yield strength YS

220 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.1E-5 1/K at 20 °C

Melting point Tm

570 °C

Specific heat capacity cp

920 J/(kg·K) at 20 °C

Thermal conductivity λ

120 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

92.1 - 95.1 %

Cu

4 - 5.2 %

Ag

0.4 - 1 %

Mn

0.2 - 0.5 %

Ti

0.15 - 0.35 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.