Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 9 g/cm³ Show Material materials with Density of 9 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 120 GPa Show Material materials with Elastic modulus of 120 GPa | |
Elongation | 23.0 °C | 20 % Show Material materials with Elongation of 20 % | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Shear modulus | 23.0 °C | 48 GPa Show Material materials with Shear modulus of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Tensile strength | 23.0 °C | 320 MPa Show Material materials with Tensile strength of 320 MPa | |
Yield strength | 23.0 °C | 280 MPa Show Material materials with Yield strength of 280 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K |
Melting point | 1080 °C Show Material materials with Melting point of 1080 °C | |
Specific heat capacity | 23.0 °C | 390 J/(kg·K) Show Material materials with Specific heat capacity of 390 J/(kg·K) |
Thermal conductivity | 23.0 °C | 390 W/(m·K) Show Material materials with Thermal conductivity of 390 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Copper | 99.99 - 100 % Show Material materials with Copper of 99.99 - 100 % |
Lead | 0 - 1E-3 % Show Material materials with Lead of 0 - 1E-3 % |
Oxygen | 0 - 5E-4 % Show Material materials with Oxygen of 0 - 5E-4 % |
Phosphorus | 0 - 3E-4 % Show Material materials with Phosphorus of 0 - 3E-4 % |