See where UNS C23000 H06 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ8.7 g/cm³ at 20 °C
Coefficient of thermal expansion
α1.9E-5 1/K at 20 °C
Melting point
Tm990 °C
Specific heat capacity
cp380 J/(kg·K) at 20 °C
Thermal conductivity
λ160 W/(m·K) at 20 °C
Electrical conductivity
σel2.15E+8 S/m at 20 °C
Element
Weight %
Comment
84 - 86 %
13.7 - 16 %
0 - 0.05 %
0 - 0.05 %
0 - 0.2 %