General
Property | Value | Temperature |
---|---|---|
Density | 8.3 g/cm³ Show Material materials with Density of 8.3 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 110 GPa Show Material materials with Elastic modulus of 110 GPa at 23.0 °C | 23.0 °C | |
Shear modulus | 40 GPa Show Material materials with Shear modulus of 40 GPa at 23.0 °C | 23.0 °C | Typical for Wrought Copper Brass |
Tensile strength | 580 MPa Show Material materials with Tensile strength of 580 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 2E-5 1/K Show Material materials with Coefficient of thermal expansion of 2E-5 1/K at 23.0 °C | 23.0 °C | |
Melting point | 875 - 1075 °C Show Material materials with Melting point of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Specific heat capacity | 390 J/(kg·K) Show Material materials with Specific heat capacity of 390 J/(kg·K) at 23.0 °C | 23.0 °C | |
Thermal conductivity | 120 W/(m·K) Show Material materials with Thermal conductivity of 120 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Copper | 61 - 64 % | |
Iron | 0 - 0.1 % | |
Lead | 0 - 0.05 % | |
Other | 0 - 0.3 % | |
Zinc | 35.6 - 39 % |