See where AA 2014 T351 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ3 g/cm³ at 23 °C
Coefficient of thermal expansion
α2.3E-5 1/K at 23 °C
Melting point
Tm510 °C
Specific heat capacity
cp870 J/(kg·K) at 23 °C
Thermal conductivity
λ150 W/(m·K) at 23 °C
Electrical conductivity
σel1.80E+7 - 3.00E+7 S/m at 23 °C
Typical for Wrought 2000 Series Aluminium
Electrical resistivity
ρel3.4E-8 - 6E-8 Ω·m at 23 °C
Typical for Wrought 2000 Series Aluminium
Element
Weight %
Comment
90.4 - 95 %
3.9 - 5 %
0.5 - 1.2 %
0.4 - 1.2 %
0.2 - 0.8 %
Workability
Moderate Workability
This material data has been provided by MakeItFrom.com.