General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 GPa Show Material materials with Elastic modulus of 200 GPa | |
Elongation | 23.0 °C | 23 % Show Material materials with Elongation of 23 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Austenitic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Austenitic Stainless Steel |
Tensile strength | 23.0 °C | 1070 MPa Show Material materials with Tensile strength of 1070 MPa | |
Yield strength | 23.0 °C | 790 MPa Show Material materials with Yield strength of 790 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K | |
Melting point | 1230 - 1480 °C Show Material materials with Melting point of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Specific heat capacity | 23.0 °C | 500 J/(kg·K) Show Material materials with Specific heat capacity of 500 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 15 W/(m·K) Show Material materials with Thermal conductivity of 15 W/(m·K) |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Electrical resistivity of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0 - 0.03 % Show Material materials with Carbon of 0 - 0.03 % |
Chromium | 16 - 18.5 % Show Material materials with Chromium of 16 - 18.5 % |
Iron | 70.2 - 77.9 % Show Material materials with Iron of 70.2 - 77.9 % |
Manganese | 0 - 2 % Show Material materials with Manganese of 0 - 2 % |
Nickel | 6 - 8 % Show Material materials with Nickel of 6 - 8 % |
Nitrogen | 0.07 - 0.2 % Show Material materials with Nitrogen of 0.07 - 0.2 % |
Phosphorus | 0 - 0.05 % Show Material materials with Phosphorus of 0 - 0.05 % |
Silicon | 0 - 1 % Show Material materials with Silicon of 0 - 1 % |
Sulfur | 0 - 0.03 % Show Material materials with Sulfur of 0 - 0.03 % |