Palladium (Pd) Half-Hard

.XLSX
.PDF
Save

Properties

General

Density ρ

11 g/cm³ at 20 °C

Mechanical

Elastic modulus E

110 GPa at 20 °C

Elongation A

1.2 % at 20 °C

Tensile strength Rm

360 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.2E-5 1/K at 20 °C

Melting point Tm

1550 °C

Specific heat capacity cp

240 J/(kg·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Pd

99.8 - 100 %

Other

0.2 %

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.