General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.4 g/cm³ Show Material materials with Density of 8.4 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 230 GPa Show Material materials with Elastic modulus of 230 GPa |
Elongation | 23.0 °C | 12 % Show Material materials with Elongation of 12 % |
Tensile strength | 23.0 °C | 960 MPa Show Material materials with Tensile strength of 960 MPa |
Yield strength | 23.0 °C | 660 MPa Show Material materials with Yield strength of 660 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K |
Specific heat capacity | 23.0 °C | 450 J/(kg·K) Show Material materials with Specific heat capacity of 450 J/(kg·K) |
Thermal conductivity | 23.0 °C | 13 W/(m·K) Show Material materials with Thermal conductivity of 13 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 0.1 % Show Material materials with Aluminium of 0 - 0.1 % |
Boron | 0 - 0.01 % Show Material materials with Boron of 0 - 0.01 % |
Carbon | 0 - 0.35 % Show Material materials with Carbon of 0 - 0.35 % |
Chromium | 27 - 30 % Show Material materials with Chromium of 27 - 30 % |
Cobalt | 58.7 - 68 % Show Material materials with Cobalt of 58.7 - 68 % |
Iron | 0 - 0.75 % Show Material materials with Iron of 0 - 0.75 % |
Manganese | 0 - 1 % Show Material materials with Manganese of 0 - 1 % |
Molybdenum | 5 - 7 % Show Material materials with Molybdenum of 5 - 7 % |
Nickel | 0 - 0.5 % Show Material materials with Nickel of 0 - 0.5 % |
Nitrogen | 0 - 0.25 % Show Material materials with Nitrogen of 0 - 0.25 % |
Phosphorus | 0 - 0.02 % Show Material materials with Phosphorus of 0 - 0.02 % |
Silicon | 0 - 1 % Show Material materials with Silicon of 0 - 1 % |
Sulfur | 0 - 0.01 % Show Material materials with Sulfur of 0 - 0.01 % |
Titanium | 0 - 0.1 % Show Material materials with Titanium of 0 - 0.1 % |
Tungsten | 0 - 0.2 % Show Material materials with Tungsten of 0 - 0.2 % |