General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.7 g/cm³ Show Material materials with Density of 8.7 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K |
Melting point | 1320 °C Show Material materials with Melting point of 1320 °C | |
Specific heat capacity | 23.0 °C | 500 J/(kg·K) Show Material materials with Specific heat capacity of 500 J/(kg·K) |
Thermal conductivity | 23.0 °C | 11 W/(m·K) Show Material materials with Thermal conductivity of 11 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Boron | 0 - 0.015 % Show Material materials with Boron of 0 - 0.015 % |
Carbon | 0 - 0.025 % Show Material materials with Carbon of 0 - 0.025 % |
Chromium | 19 - 21 % Show Material materials with Chromium of 19 - 21 % |
Cobalt | 29.1 - 39 % Show Material materials with Cobalt of 29.1 - 39 % |
Iron | 0 - 1 % Show Material materials with Iron of 0 - 1 % |
Manganese | 0 - 0.15 % Show Material materials with Manganese of 0 - 0.15 % |
Molybdenum | 9 - 10.5 % Show Material materials with Molybdenum of 9 - 10.5 % |
Nickel | 33 - 37 % Show Material materials with Nickel of 33 - 37 % |
Phosphorus | 0 - 0.02 % Show Material materials with Phosphorus of 0 - 0.02 % |
Silicon | 0 - 0.15 % Show Material materials with Silicon of 0 - 0.15 % |
Sulfur | 0 - 0.01 % Show Material materials with Sulfur of 0 - 0.01 % |
Titanium | 0 - 1 % Show Material materials with Titanium of 0 - 1 % |