Custom 450 Bar

Alternative and trade names
AISI XM-25, UNS S45000
.XLSX
.PDF
Save

Description

Related Standards

Chemical properties

Element

Weight %

Comment

Fe

-

Bal

Other

-

Columbium 8x min carbon

Cr

14 - 16 %

Ni

5 - 7 %

Cu

1.25 - 1.75 %

More