Titanium Gr. 5 Bar

Alternative and trade names
UNS R56400, AMS 4911, AMS 4920, AMS 4928, 3.7164, 3.7165, MIL 9046, MIL 9047, AFNOR T-A6V
.XLSX
.PDF
Save

Description

Related Standards

Chemical properties

Element

Weight %

Comment

Ti

87.98 %

Al

5.5 - 6.75 %

V

3.5 - 4.5 %

Fe

0.4 %

C

0.1 %

More

This material data has been provided by MMC-LTD.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.