The material: 'StarCeram® AT Aluminium Titanate 1201 (Al₂TiO₅)' you were looking for has been superseded by the one below.

Aluminium Titanate (KTiAl)

Want to keep this datasheet? Save it now in your required format

Description

Nanoker produces ceramic components and tailor made products from KTiAl. The key benefits of Aluminium Titanate (KTiAl) are: Excellent thermal shock resistance, good corrosion resistance, good insulating properties, good wear resistance, very low wettability by non-ferrous melts.

This material data has been provided by Nanoker.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

3.1 g/cm³

Show Supplier Material materials with Density of 3.1 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

20 GPa

Show Supplier Material materials with Elastic modulus of 20 GPa

Flexural strength

23.0 °C

30 MPa

Show Supplier Material materials with Flexural strength of 30 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

1000.0 °C

1.5E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.5E-6 1/K

Max service temperature, continuous

1100 °C

Show Supplier Material materials with Max service temperature, continuous of 1100 °C

Max service temperature, intermittent

1350 °C

Show Supplier Material materials with Max service temperature, intermittent of 1350 °C

Thermal conductivity

23.0 °C

2 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 2 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

1.00E+11 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.00E+11 Ω·m

Chemical properties

PropertyValueComment

Aluminium

56.5 %

Show Supplier Material materials with Aluminium of 56.5 %

as Al₂O₃

Iron

0.02 %

Show Supplier Material materials with Iron of 0.02 %

as Fe₂O₃

Silicon

0.01 %

Show Supplier Material materials with Silicon of 0.01 %

as SiO₂

Sodium

0.05 %

Show Supplier Material materials with Sodium of 0.05 %

as Na₂O

Titanium

41.26 %

Show Supplier Material materials with Titanium of 41.26 %

as TiO₂

Zirconium

1 %

Show Supplier Material materials with Zirconium of 1 %

as ZrO₂ + HfO₂

Technological properties

Property
Application areas

Typical application areas include: Foundries, non-ferrous metal forming industry, labware