Glass cord A13-080149 / A13-080249

Want to keep this datasheet? Save it now in your required format

Description

Chloroprene latex impregnated E glass cord (Elastomer Polymer Matrix Composite)

Properties

General

Adhesion

Fad

125 N at 20 °C

min., Hot U Test

Linear density

ρlinear

0.01 g/cm at 20 °C

Dimension

Bobbin Inner Diameter

db,i

60 mm

Bobbin Length

lb

356 mm

Flange Diameter

Df

159 mm

Mechanical

Nominal breaking force

Fb

667 N at 20 °C

Show Aluminosilicate materials with Nominal breaking force of 667 N at 20 °C

Tensile Member: E Glass

Technological properties

Color

Black

Cord Construction

330.1/0

Other

Manufacturing Location: Canada

Processing history

Latex Type: Chloroprene, Dip Pick-Up: 19 to 28%

Twist per Meter

TPM

70 - 90 TPM

Direction: S & Z

This material data has been provided by NGF Glass.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.