Description

Designed for Processing in Laser Powder Bed Fusion (PBF-LB), Electron Beam Powder Bed Fusion (PBF-EB) or Directed Energy Deposition (DED) Systems



MetcoAdd™ 17-4PH is a family of martensitic, precipitation-hardening stainless steel powders with chemistry similar to AMS 5643. 


Room temperature static properties of PBF-LB processed and heat treated material coupons have been shown to be comparable to those of AMS 5643 in the H900 state. 


For reference purposes Oerlikon has processed MetcoAdd 17-4PH-A using fixed parameters and 40 μm layer thickness to provide data below. Additional testing has been performed by an extensive network of consortia and customer partners on a broader range of machine types. Properties may be optimized based on application specific requirements

Related Standards

Properties

General

Density ρ

4 g/cm³ at 20 °C

typical apparent density, min

Hall flow HF

16 s/50g at 20 °C

ASTM B213, max MetcoAdd 17-4PH-A

Morphology

Spheroidal

Particle size D10 D10

19 μm

nominal values by laser diffraction; MetcoAdd 17-4PH-A

Particle size D50 D50

30 μm

nominal values by laser diffraction; MetcoAdd 17-4PH-A

Particle size D90 D90

45 μm

nominal values by laser diffraction; MetcoAdd 17-4PH-A

Particle size range drange

15 - 45 µm

ASTM C 1070 (Microtrac); MetcoAdd 17-4PH-A: -45 +15μm; MetcoAdd 17-4PH-D: -106 +45μm

Thermal

Melting point Tm

1456 - 1491 °C

± 10 °C

Chemical properties

Element

Weight %

Comment

Fe

-

balance

Cr

17 %

Ni

4.5 %

Cu

4 %

Other

1 %

max

More

Technological properties

Application areas

Aerospace, Chemical processing, Nuclear and oil / petrochemical refining, General metalworking, Surgical parts

Availability

Stock

Chemical composition

FeCrNiCu

Distribution

Global

Handling recommendations

Blend contents prior to use to prevent segregation; Keep in the original container, or an approved alternative, tightly closed when not in use; Powder from previously opened containers should be stored in a humidity-controlled environment

Order number

17-4PH-A: 1093744, 17-4PH-D: 1305324

Packaging size

4.5 kg / 10 lb approx.

Processing history

Gas atomized (Argon)

Processing methods

Laser Powder Bed Fusion (PBF-LB), Electron Beam Powder Bed Fusion (PBF-EB), Directed Energy Deposition (DED)

Safety data sheet

www.oerlikon.com/metco SDS No.50-2005

This material data has been provided by Oerlikon AM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.