230 Nickel Alloy for Laser Powder Bed Fusion (PBF-LB)

Alternative and trade names
MetcoAdd™ H230-A
.XLSX
.PDF
Save

Description

Designed for Processing in Laser Powder Bed Fusion (PBF-LB) Systems


MetcoAdd™ H230-A is a nickel-based powder product with chemistry similar to AMS 5891 bar material. 


Room temperature static properties of PBF-LB processed and heat treated material coupons have been shown to be comparable to those of AMS 5891. Elevated temperature tensile and creep rupture data may be made available upon request. 


For reference purposes Oerlikon has processed MetcoAdd H230-A using 40 μm layer thickness to provide data below. Properties may be optimized based on application specific requirements.

Related Standards

Properties

General

Density ρ

4.5 - 5 g/cm³ at 20 °C

typical apparent density

Hall flow HF

20 s/50g at 20 °C

ASTM B213, max (typical)

Morphology

Spheroidal

Particle size D10 D10

25 μm

nominal values by laser diffraction

Particle size D50 D50

35 μm

nominal values by laser diffraction

Particle size D90 D90

49 μm

nominal values by laser diffraction

Particle size range drange

15 - 45 µm

ASTM C 1070 (Microtrac)

Thermal

Melting point Tm

1327 - 1455 °C

± 10 °C

Chemical properties

Element

Weight %

Comment

Ni

-

balance

Cr

20 - 24 %

W

13 - 15 %

Co

5 %

max

Fe

3 %

max

More

Technological properties

Application areas

Aerospace: Engine components, Power Generation: Gas turbine components, Industrial: Components requiring high temperature corrosion resistance for chemical, metallurgical and mineral process industries

Availability

Stock

Chemical composition

NiCrWMoAlTi

Distribution

Global

Handling recommendations

Blend contents prior to use to prevent segregation; Keep in the original container, or an approved alternative, tightly closed when not in use; Powder from previously opened containers should be stored in a humidity-controlled environment

Order number

1300725

Packaging size

4.5 kg/ 10 lb approx.

Processing history

Gas atomized (Argon)

Processing methods

Laser Powder Bed Fusion (PBF-LB)

Safety data sheet

www.oerlikon.com/metco SDS No. 50-2122

This material data has been provided by Oerlikon AM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.