316L Stainless Steel for Laser Powder Bed Fusion (PBF-LB), Electron Beam Powder Bed Fusion (PBF-EB) or Directed Energy Deposition (DED)

Alternative and trade names
MetcoAdd™ 316L-A, MetcoAdd™ 316L-D
.XLSX
.PDF
Save

Description

Designed for Processing in Laser Powder Bed Fusion (PBF-LB), Electron Beam Powder Bed Fusion (PBF-EB) or Directed Energy Deposition (DED) Systems 


MetcoAdd™ 316L is a family of austenitic steel powders with chemistry similar to EN 1.4404 and UNS S316603.


Room temperature static properties of PBF-LB processed, as-built, material coupons have been shown to be comparable to those of AMS 5424. 


For reference purposes Oerlikon has processed MetcoAdd 316L-A using fixed parameters and 40 μm layer thickness to provide data below. Additional testing has been performed by an extensive network of consortia and customer partners on a broader range of machine types. Properties may be optimized based on application specific requirements.

Related Standards

Properties

General

Density ρ

4 g/cm³ at 20 °C

typical apparent density, min

Hall flow HF

20 s/50g at 20 °C

ASTM B213, max MetcoAdd 316L-A

Morphology

Spheroidal

Particle size D10 D10

19 μm

nominal values by laser diffraction, MetcoAdd 316L-A

Particle size D50 D50

30 μm

nominal values by laser diffraction, MetcoAdd 316L-A

Particle size D90 D90

46 μm

nominal values by laser diffraction, MetcoAdd 316L-A

Particle size range drange

15 - 45 µm

ASTM C 1070 (Microtrac); MetcoAdd™ 316L-A: -45 +15µm; MetcoAdd™ 316L-D: -106 +45µm

Thermal

Melting point Tm

1390 - 1448 °C

± 10 °C

Chemical properties

Element

Weight %

Comment

Fe

-

balance

Cr

18 %

Ni

12 %

Mo

2 %

Other

1 %

max

More

Technological properties

Application areas

Aerospace: Clamping elements and heat exchangers, Medical: Surgical tools and orthopedic implants, Transport: Maritime components, Tooling: Pressure injection dies and molds, Consumer: Jewelry and watch components

Availability

Stock

Chemical composition

FeCrNiMoC

Distribution

Global

Handling recommendations

Blend contents prior to use to prevent segregation; Keep in the original container, or an approved alternative, tightly closed when not in use; Powder from previously opened containers should be stored in a humidity-controlled environment

Order number

316L-A: 1093739, 316L-D: 1305325

Packaging size

316L-A: 4.5 kg / 10 lb approx., 316L-D: 4.5 kg / 10 lb approx.

Processing history

Gas atomized (Nitrogen)

Processing methods

Laser Powder Bed Fusion (PBF-LB), Electron Beam Powder Bed Fusion (PBF-EB), Directed Energy Deposition (DED)

Safety data sheet

www.oerlikon.com/metco SDS No.50-1990

This material data has been provided by Oerlikon AM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.