718 Nickel Alloy for Laser Powder Bed Fusion (PBF-LB), Electron Beam Powder Bed Fusion (PBF-EB) or Directed Energy Deposition (DED) Systems

Alternative and trade names
MetcoAdd™ 718C, MetcoAdd™ 718E, MetcoAdd™ 718F, MetcoAdd™ 718G
.XLSX
.PDF
Save

Description

Designed for Processing in Laser Powder Bed Fusion (PBF-LB), Electron Beam Powder Bed Fusion (PBF-EB) or Directed Energy Deposition (DED) Systems 


MetcoAdd™ 718 is a family of nickel-based superalloy powders with chemistry similar to AMS 5662 bar material. 


Room temperature static properties of PBF-LB processed and heat treated material coupons have been shown to be comparable to those of AMS 5662. 


For reference purposes Oerlikon has processed MetcoAdd 718C using fixed parameters and 40 μm layer thickness to provide data below. Additional testing has been performed by an extensive network of consortia and customer partners on a broader range of machine types. Properties may be optimized based on application specific requirements.

Related Standards

Properties

General

Density ρ

4 - 5 g/cm³ at 20 °C

typical apparent density

Hall flow HF

18 s/50g at 20 °C

ASTM B213, max MetcoAdd 718C

Morphology

Spheroidal

Particle size D10 D10

18 μm

nominal values by laser diffraction; MetcoAdd 718C

Particle size D50 D50

30 μm

nominal values by laser diffraction; MetcoAdd 718C

Particle size D90 D90

46 μm

nominal values by laser diffraction; MetcoAdd 718C

Particle size range drange

15 - 45 µm

ASTM C 1070 (Microtrac); MetcoAdd 718C: -45 +15µm; MetcoAdd 718E: -63 +20µm; MetcoAdd 718F: -106 +45µm; MetcoAdd 718G: -90 +45µm

Thermal

Melting point Tm

1260 - 1340 °C

± 10 °C

Chemical properties

Element

Weight %

Comment

Ni

-

balance

Cr

18 %

Fe

18 %

Nb+Ta

5 %

Mo

3 %

More

Technological properties

Application areas

Aerospace: Engine components; Power Generation: Gas turbine components; Oil & Gas: Sensors; Industrial: Various

Availability

718C: stock; 718E: special order; 718F: stock; 718G: stock

Chemical composition

NiCrMo[Fe](Nb+Ta)AlTi

Distribution

Global

Handling recommendations

Blend contents prior to use to prevent segregation; Keep in the original container, or an approved alternative, tightly closed when not in use; Powder from previously opened containers should be stored in a humidity-controlled environment

Order number

718C: 1096973, 718E: 1100779, 718F: 1305326, 718G: 1305327

Packaging size

718C: 2.25 kg / 5 lb approx.; 718E: 4.5 kg / 10 lb approx.; 718F: 4.5 kg / 10 lb approx.; 718G: 4.5 kg / 10 lb approx.

Processing history

Gas atomized (Argon)

Processing methods

Laser Powder Bed Fusion (PBF-LB), Electric Beam Powder Bed Fusion (PBF-EB), Directed Energy Deposition (DED)

Safety data sheet

www.oerlikon.com/metco SDS No.50-1957

This material data has been provided by Oerlikon AM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.