Description

Designed for Processing in Laser Powder Bed Fusion (PBF-LB) Systems


MetcoAdd™ H11-A is martensitic, iron-chromium, air-hardenable steel powder product with chemistry similar to UNS T20811, ASTM A681, SAE J437, AMS 6487 and Werkstoff No. 1.2343 / X37CrMoV 5-1. 


Room temperature static properties of PBF-LB processed and heat treated material coupons have been shown to be comparable to those of AMS 6487.

Related Standards

Properties

General

Density ρ

4 g/cm³ at 20 °C

typical apparent density, min

Hall flow HF

20 s/50g at 20 °C

ASTM B213, max

Morphology

Spheroidal

Particle size D10 D10

21 μm

nominal values by laser diffraction

Particle size D50 D50

34 μm

nominal values by laser diffraction

Particle size D90 D90

50 μm

nominal values by laser diffraction

Particle size range drange

15 - 45 µm

ASTM C 1070 (Microtrac)

Thermal

Melting point Tm

1371 - 1482 °C

Chemical properties

Element

Weight %

Comment

Fe

-

balance

Cr

4.75 - 5.5 %

Mo

1.1 - 1.6 %

Si

0.8 - 1.25 %

C

0.33 - 0.43 %

More

Technological properties

Application areas

Highly stressed structural parts, e.g. aircraft landing gears, hot forging and extrusion dies, helicopter rotor blades, die casting molds

Availability

Stock

Chemical composition

Fe 5Cr 1Mo 1Si 0.5V 0.4C

Distribution

Global

Handling recommendations

Blend contents prior to use to prevent segregation; Keep in the original container, or an approved alternative, tightly closed when not in use; Powder from previously opened containers should be stored in a humidity-controlled environment

Order number

1305824

Packaging size

4.5kg / 10 lb approx.

Processing history

Gas atomized (Argon)

Processing methods

Laser Powder Bed Fusion (PBF-LB)

Safety data sheet

www.oerlikon.com/metco SDS No. 50-2354

This material data has been provided by Oerlikon AM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.