Show me around

SANI-ETHYLENE™ PE0014

Want to keep this datasheet? Save it now in your required format

Description

General Purpose low density polyethylene with antibacterial efficacy greater than 99% according to ISO 22196.

Properties

General

Density

ρ

0.92 g/cm³ at 20 °C

ISO 1183

Melt mass-flow rate

MFR

0.25 g/10min at 20 °C

ISO 1133

Thermal

Melting point

Tm

110 °C

ISO 11357-3

Technological properties

Application areas

Suitable for food packaging materials and food packaging films. Perfectly suitable to blend in with other grades of polyethylene.

Other

Mixing ratio 3:97

Processing methods

Extrusion, multilayer processing, injection molding

Do you need more data regarding this material?

This material data has been provided by Parx Plastics.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.