Show me around

SANI-ETHYLENE™ PE0002

Want to keep this datasheet? Save it now in your required format

Description

General Purpose linear low density polyethylene wit antibacterial efficacy of 97-99% according to ISO 22196.

Properties

General

Density

ρ

0.92 g/cm³ at 23 °C

ISO 1872-1

Melt mass-flow rate

MFR

2.1 g/10min at 20 °C

ISO 1133

Technological properties

Application areas

Suitable for food packaging materials and food packaging films. Perfectly suitable to blend in with other grades of polyethylene.

Other

Mixing ratio 6:94

Processing methods

Extrusion, multilayer processing, injection molding

Do you need more data regarding this material?

This material data has been provided by Parx Plastics.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.