General Purpose high molecular weight polystyrene with antibacterial efficacy of 97-99% according to ISO 22196.

Properties

General

Density

ρ

1.05 g/cm³ at 20 °C

ISO 1183

Melt mass-flow rate

MFR

2.5 g/10min at 200 °C

tested with 5 kg load according to ISO 1133

Technological properties

Application areas

General Purpose grade very suited for packaging applications.

Other

Mixing ratio 1:99

Processing methods

Extrusion blending