Description

General Purpose acrylonitrile butadiene styrene with easy flow, medium impact and antibacterial efficacy greater than 99% according to ISO 22196.

Properties

General

Melt mass-flow rate MFR

3.8 - 46 g/10min at 200 °C

tested with 5, 10 and 21.6 kg loads respectively according to ASTM D1238

Technological properties

Other

Mixing ratio 3:97

This material data has been provided by Parx Plastics.