PHOENIX™ 01101 fully hydrogenated SEBS (Styrene Ethylene Butylene Styrene) compound

Alternative and trade names
THERMOLAST®, Monprene®, Versaflex™, Dryflex®
Want to keep this datasheet? Save it now in your required format

Description

This grade is an easy processing Thermoplastic Elastomer (TPE) designed for injection molding applications that have FDA requirements. The key features are: Soft touch, easy to process and color, rubber like texture and feel, excellent weather resistance, excellent tensile strength, excellent elasticity, meet FDA requirements

Properties

General

Density

ρ

0.83 - 0.89 g/cm³ at 20 °C

ASTM D792

Melt mass-flow rate

MFR

11.2 g/10min at 20 °C

ASTM D1238 (190°C, 1.2kg)

Shrinkage

cshrink

2.3 - 2.9 % at 20 °C

ASTM D955

Shrinkage, transverse

cshrink, trans

2.2 - 2.8 % at 20 °C

ASTM D955

Mechanical

Elongation

A

1101 % at 20 °C

ASTM D412 (500 mm/min)

Hardness, Shore A

HS A

7 - 13 [-] at 20 °C

ASTM D2240

Modulus at 100% elongation

EA=100

1.59159E-4 GPa at 20 °C

ASTM D412 (500 mm/min)

Modulus at 300% elongation

EA=300

2.38394E-4 GPa at 20 °C

ASTM D412 (500 mm/min)

Tear strength

Rtear

8.83 kN/m at 20 °C

ASTM D624 Die C (500 mm/min)

Tensile strength

Rm

2.7 MPa at 20 °C

ASTM D412 (500 mm/min)

Technological properties

Application areas

Shoes insole, medical appliances, fishing lure, sports equipment, toys

Color

Transparent

Processing Tag

This material data has been provided by Phon Tech.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.