General
Property | Value | Testing Standard |
---|---|---|
Density | 0.82 - 0.88 g/cm³ Show Supplier Material materials with Density of 0.82 - 0.88 g/cm³ | ASTM D792 |
Mechanical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elongation | 1100.6 % Show Supplier Material materials with Elongation of 1100.6 % | ASTM D412 | 500 mm/min |
Modulus at 100% elongation | 6e-05 GPa Show Supplier Material materials with Modulus at 100% elongation of 6e-05 GPa | ASTM D412 | 500 mm/min |
Modulus at 300% elongation | 0.0001 GPa Show Supplier Material materials with Modulus at 300% elongation of 0.0001 GPa | ASTM D412 | 500 mm/min |
Tear strength | 2.1 kN/m Show Supplier Material materials with Tear strength of 2.1 kN/m | ASTM D624 Die C | 500 mm/min |
Tensile strength | 0.603 MPa Show Supplier Material materials with Tensile strength of 0.603 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 353.3 g/10min Show Supplier Material materials with Melt mass-flow rate of 353.3 g/10min | ASTM D1238 | 190°C/1.2kg |
Shrinkage | 2.2 - 2.8 % Show Supplier Material materials with Shrinkage of 2.2 - 2.8 % | ASTM D955 | Transverse |
3 - 3.6 % Show Supplier Material materials with Shrinkage of 3 - 3.6 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Rehabilitation ball, sticker toys, fishing bait, personal care | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Transparent |