Property | Value | Testing Standard |
---|---|---|
Density | 1.02 - 1.08 g/cm³ Show Supplier Material materials with Density of 1.02 - 1.08 g/cm³ | ASTM D792 |
Mechanical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elongation | 640 % Show Supplier Material materials with Elongation of 640 % | ASTM D412 | 500 mm/min |
Hardness, Shore A | 17 - 23 [-] Show Supplier Material materials with Hardness, Shore A of 17 - 23 [-] | ASTM D2240 | |
Modulus at 100% elongation | 0.00047 GPa Show Supplier Material materials with Modulus at 100% elongation of 0.00047 GPa | ASTM D412 | 500 mm/min |
Modulus at 300% elongation | 0.00081 GPa Show Supplier Material materials with Modulus at 300% elongation of 0.00081 GPa | ASTM D412 | 500 mm/min |
Tear strength | 7.2 kN/m Show Supplier Material materials with Tear strength of 7.2 kN/m | ASTM D624 Die C | 500 mm/min |
Tensile strength | 1.5 MPa Show Supplier Material materials with Tensile strength of 1.5 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 50.8 g/10min Show Supplier Material materials with Melt mass-flow rate of 50.8 g/10min | ASTM D1238 | 190°C/1.2kg |
Shrinkage | 0.9 - 1.5 % Show Supplier Material materials with Shrinkage of 0.9 - 1.5 % | ASTM D955 | |
0.9 - 1.5 % Show Supplier Material materials with Shrinkage of 0.9 - 1.5 % | ASTM D955 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Bicycle grip, tool grip, toothbrush | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |