General
Property | Value | Testing Standard |
---|---|---|
Density | 0.96 - 1.02 g/cm³ Show Supplier Material materials with Density of 0.96 - 1.02 g/cm³ | ASTM D792 |
Mechanical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elongation | 586.4 % Show Supplier Material materials with Elongation of 586.4 % | ASTM D412 | 500 mm/min |
Hardness, Shore D | 49 - 55 [-] Show Supplier Material materials with Hardness, Shore D of 49 - 55 [-] | ASTM D2240 | |
Modulus at 100% elongation | 0.0134 GPa Show Supplier Material materials with Modulus at 100% elongation of 0.0134 GPa | ASTM D412 | 500 mm/min |
Modulus at 300% elongation | 0.0135 GPa Show Supplier Material materials with Modulus at 300% elongation of 0.0135 GPa | ASTM D412 | 500 mm/min |
Tear strength | 115.7 kN/m Show Supplier Material materials with Tear strength of 115.7 kN/m | ASTM D624 Die C | 500 mm/min |
Tensile strength | 16.1 MPa Show Supplier Material materials with Tensile strength of 16.1 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 11.4 g/10min Show Supplier Material materials with Melt mass-flow rate of 11.4 g/10min | ASTM D1238 | 190°C/2.16kg |
Shrinkage | 0.8 - 1.4 % Show Supplier Material materials with Shrinkage of 0.8 - 1.4 % | ASTM D955 | Transverse |
0.9 - 1.5 % Show Supplier Material materials with Shrinkage of 0.9 - 1.5 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Cosmetics, battery seal | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | White | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |