General
Property | Value | Testing Standard |
---|---|---|
Density | 0.94 - 1 g/cm³ Show Supplier Material materials with Density of 0.94 - 1 g/cm³ | ASTM D792 |
Mechanical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elongation | 980.4 % Show Supplier Material materials with Elongation of 980.4 % | ASTM D412 | 500 mm/min |
Hardness, Shore A | 57 - 63 [-] Show Supplier Material materials with Hardness, Shore A of 57 - 63 [-] | ASTM D2240 | |
Modulus at 100% elongation | 0.00154 GPa Show Supplier Material materials with Modulus at 100% elongation of 0.00154 GPa | ASTM D412 | 500 mm/min |
Modulus at 300% elongation | 0.00239 GPa Show Supplier Material materials with Modulus at 300% elongation of 0.00239 GPa | ASTM D412 | 500 mm/min |
Tear strength | 28.6 kN/m Show Supplier Material materials with Tear strength of 28.6 kN/m | ASTM D624 Die C | 500 mm/min |
Tensile strength | 8.4 MPa Show Supplier Material materials with Tensile strength of 8.4 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 4.9 g/10min Show Supplier Material materials with Melt mass-flow rate of 4.9 g/10min | ASTM D1238 | 190°C/5kg |
Shrinkage | 1.4 - 2 % Show Supplier Material materials with Shrinkage of 1.4 - 2 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Shrinkage of 1.5 - 2.1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Syringe gasket, sport products, tool grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Bio-Compatible | |
Color | Black | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |