PHOENIX™ 04551 fully hydrogenated SEBS (Styrene Ethylene Butylene Styrene) compound

Alternative and trade names
THERMOLAST®, Monprene®, Versaflex™, Dryflex®
.XLSX
.PDF
Save

Description

This grade is designed for extrusion and injection molding applications that have FDA requirements. The key features are: Soft touch, excellent scratch endurance, easy to process and color, excellent tensile strength, good elasticity, excellent weather resistance, good appearance, meet FDA requirements

Properties

General

Density ρ

0.85 - 0.91 g/cm³ at 20 °C

ASTM D792

Melt mass-flow rate MFR

6.9 g/10min at 20 °C

ASTM D1238 (200°C, 5kg)

Shrinkage cshrink

1.5 - 2.1 % at 20 °C

ASTM D955

Shrinkage, transverse cshrink, trans

1.4 - 2 % at 20 °C

ASTM D955

Mechanical

Elongation A

768.4 % at 20 °C

ASTM D412 (500 mm/min)

Hardness, Shore A HS A

52 - 58 [-] at 20 °C

ASTM D2240

Modulus at 100% elongation EA=100

1.32977E-3 GPa at 20 °C

ASTM D412 (500 mm/min)

Modulus at 300% elongation EA=300

2.468687E-3 GPa at 20 °C

ASTM D412 (500 mm/min)

Tear strength Rtear

29.42 kN/m at 20 °C

ASTM D624 Die C (500 mm/min)

Tensile strength Rm

6.21 MPa at 20 °C

ASTM D412 (500 mm/min)

Technological properties

Application areas

Extrusion profile, tube

Color

Translucent

Processing methods

Injection molding, extrusion

This material data has been provided by Phon Tech.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.