Description

This grade is an easy processing Thermoplastic Elastomer (TPE) designed for injection molding applications that have FDA requirements. The key features are: Excellent scratch endurance, easy to process and color, excellent tensile strength, good elasticity, excellent weather resistance, good appearance, overmoldable to Polypropylene, meet FDA requirements

This material data has been provided by Phon Tech.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTesting Standard

Density

0.85 - 0.91 g/cm³

Show Supplier Material materials with Density of 0.85 - 0.91 g/cm³

ASTM D792

Mechanical

PropertyValueTesting StandardComment

Elongation

1051.9 %

Show Supplier Material materials with Elongation of 1051.9 %

ASTM D412

500 mm/min

Hardness, Shore A

62 - 68 [-]

Show Supplier Material materials with Hardness, Shore A of 62 - 68 [-]

ASTM D2240

Modulus at 100% elongation

0.00293 GPa

Show Supplier Material materials with Modulus at 100% elongation of 0.00293 GPa

ASTM D412

500 mm/min

Modulus at 300% elongation

0.00413 GPa

Show Supplier Material materials with Modulus at 300% elongation of 0.00413 GPa

ASTM D412

500 mm/min

Tear strength

47.7 kN/m

Show Supplier Material materials with Tear strength of 47.7 kN/m

ASTM D624 Die C

500 mm/min

Tensile strength

9.4 MPa

Show Supplier Material materials with Tensile strength of 9.4 MPa

ASTM D412

500 mm/min

Rheological Properties

PropertyValueTesting StandardComment

Melt mass-flow rate

16.1 g/10min

Show Supplier Material materials with Melt mass-flow rate of 16.1 g/10min

ASTM D1238

200°C/5kg

Shrinkage

1.4 - 2 %

Show Supplier Material materials with Shrinkage of 1.4 - 2 %

ASTM D955

Transverse

1.5 - 2.1 %

Show Supplier Material materials with Shrinkage of 1.5 - 2.1 %

ASTM D955

Technological properties

Property
Application areas

Cap liner

Certifications

REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements, Bio-Compatible

Color

Translucent

Other

Overmolding capabilities: PP